The direct oxidation of toluene to cresols with nitrous oxide as the oxidant was carried out over a ZSM-5 zeolite catalyst under gaseous and supercritical conditions (395 °C and 0.5, 7, 12 MPa; 420 °C and 15 MPa). The supercritical oxidation is characterized by a significantly greater productivity as compared to the gas-phase process. Successful in situ regeneration of the deactivated catalyst during the transition from the gas-phase to the supercritical process has been demonstrated.
Cite:
Bogdan V.I.
, Zholobenko V.L.
, Bogdan T.V.
, Kustov A.L.
, Koklin A.E.
, Mishanin I.I.
, Mashchenko N.V.
, Bogorodskiy S.E.
Oxidation of toluene with N2O on ZSM-5 zeolite under supercritical conditions
Mendeleev Communications. 2025. V.35. N3. P.344-346. DOI: 10.71267/mencom.7626 WOS OpenAlex
Oxidation of toluene with N2O on ZSM-5 zeolite under supercritical conditions
Mendeleev Communications. 2025. V.35. N3. P.344-346. DOI: 10.71267/mencom.7626 WOS OpenAlex
Identifiers:
| Web of science: | WOS:001490937900003 |
| OpenAlex: | W4409003309 |
Citing:
Пока нет цитирований