Preparation and thermal behavior of the formulation of Ftorsam-39 with SKF-26(ONM) fluorine rubber Full article

Journal Russian Chemical Bulletin
ISSN: 1573-9171 , E-ISSN: 1066-5285
Output data Year: 2019, Volume: 68, Number: 2, Pages: 449-452 Pages count : 4 DOI: 10.1007/s11172-019-2407-5
Authors Sakharov A.M. 1 , Popovich M.Yu. 1 , Krukovsky S.P. 1
Affiliations
1 N. D. Zelinsky Institute of Organic Chemistry Russian Academy of Science, 47 Leninsky prosp., 119991, Moscow, Russian Federation

Abstract: A synthetic procedure was designed to prepare formulations from Ftorsam-39 monomer (perfluoro-2,5-dimethyl-3,6-dioxanonoic acid triethoxysilylpropylamide) with SKF-26(ONM) fluorine rubber (poly(vinylidene fluoride-co-hexafluoropropylene)) in a presence of AGM-9 (γ-aminopropyltriethoxysilane) as a catalyst and co-reagent. The content of fluorine rubber in the compositions was varied from 10 to 54 wt.%. Thermal properties of the formulations obtained with the ratio Ftorsam-39: SKF-26(ONM): AGM-9 = 40: 54: 6 (wt.%) were assessed using thermomechanical and thermogravimetric analysis and differential scanning calorimetry.
Cite: Sakharov A.M. , Popovich M.Y. , Krukovsky S.P.
Preparation and thermal behavior of the formulation of Ftorsam-39 with SKF-26(ONM) fluorine rubber
Russian Chemical Bulletin. 2019. V.68. N2. P.449-452. DOI: 10.1007/s11172-019-2407-5 WOS Scopus OpenAlex